Chemical CompositionPolyethylene WaxTechnical ParametersNature of theProductPEW-0205BAppearance White PowderParticle Size μmDv50 7Dv90 18Melting Point â 110Characteristics and Purposesà Micronized wax which is suitable forsolvent-based flexo-printing ink, as well assolvent-based gravure printing ink, can improvethe abrasion resistance, and scratch resistancewhen used in solvent-based ink. PEW-0205Bcan reduce the coefficient of friction in differentkinds of inks. Whatâs more, PEW-0205B hasgood adaptability in benzene soluble ink,alcohol soluble ink and resin soluble ink.à In offset ink, PEW-0205B can obviouslyincrease the abrasion resistance of layer, and theadditive amount is normally at 0.5-1%.à PEW-0205B can improve the abrasionresistance, scratch resistance in varieties ofcoatings. Can also be used in plastics coatings,coil coatings and other fields as well assolvent-based ink.à Can be used in powder coating, to improvethe hardness and scratch resistance at theadditive amount of 0.3%, and will notsmoke under 180â baking.Additive amount and Usageà In varieties of systems, the additionalamount of the micronized wax is generallybetween 0.5 to 3%.à Usually by a direct high-speed stirring, itcan disperse in solvent-based coatings andprinting inks.à It can be added by using varieties ofgrinding machines, high-shear dispersingdevice, and grind mill. Should payattention to the temperature control.à Can make wax slurry with the wax at20-30%, and add it into the systems whenneeded, by which the wax dispersion timecan be saved.Packaging and Storageà Paper-plastic bag, net weight: 20 kg / bag.à This product is non-dangerous goods.Please store it away from ignition sourcesand strong oxidants.