Thing | Block | Index | Test condition | |
Thickness | Um | 12 | ||
Tensile strength | MD | MPa | 216 | Temperature: 23 âRelative humidity40% |
TD | MPa | 205 | ||
Elongation atBreak | MD | % | 115 | |
TD | % | 102 | ||
Coefficient of friction | ----- | 0.56 | ||
Equality aluminized layer | % | ± 5 | ||
Speed ââaluminized layer | % | No al husk layer | ||
Wetting the tension of the aluminum layer | MN / m | 54 | ||
Aluminized layer thickness | A | 100 |