BAISC INFORMATION | |
A. Product Name | Colorful Non-slip Thermoplastic Road Marking Paint |
B. Use For | Concrete and aslt floor |
C. Components | Resin, Rubber Elastomer, Ceramic Particle |
D. Appearance | Powder |
E. Standard | JT/T280-2004 |
F. Color | White, yellow, Red, Blue, Green, Black (OEM) |
G. Weight | 25kg/bag |
H. Density | 2.01/ cm³ |
I. Film Thickness | 1.8-2.0mm |
SICAL CHARACTERISTICS | |
A. Compression Strength | 23.8MPa |
B. Fluidity | 38 |
C. Abrasion Resistance | 56.8 |
D. Glass Beads | 0% |
E. Softening Temperature | 104°C |
F. Heating Temperature | 180-200°C |
G. Drying Time After Marking | Touch dry—3 mins |
Full dry—10 mins | |
H. Shelf Life | Up to 24 months |
I. Storage | Store in a tightly sealed container in a cool & dry place |
J. Area Of n> | 1 Ton thermoplastic paint can mark about 125 m2 |
FEATURES |
A. High usage ratio |
B. Save the cost of gas |
C. Exnt durability |
D. Strong adhesion power |
E. High dirty pick-up resistance |
F. Not faded easily marking n> |
G. Bright-colors makes road more beautiful and distinct |
H. It highly improves the non-slip effect |
I. Car will vibrate when it passes through the marking n> |
RECOMMENDATION | |
A. Equipment | Pre-heater |
Thermoplastic road marking machine | |
Primer sprayer | |
Road blower | |
Road sprayer | |
B. Dosage Ratio | Thermoplastic paint: 1Ton |
Primer: 20KG | |
Glass beads: 50KG |
PROCESS | |
A. Clean | Clean intended application area thorough |
B. Layout | Outarea where the marking will be placed using titanium dioxide |
C. Apply primer | Apply the appropriate amount of primer needed for the surface |
D. Melt | Heat paint to be melted using pre-heater |
E. Position A | Pour melted paint into big container of road marking machine |
Position B | Pour glass beads into small container of road marking machine |
F. Mark | Mark thermoplastic g road marking machine |
G. Cool | Thermoplastic cool within a period of time |
ATTENTION |
A. Ensure road surface is stable, dry and clean |
B. It is better to apply above 0°C |
C. Heating paint in the pre-heater should be between 180-200 °C |
D. Lift the heating temperature properly when working in a low temperature environment |
E. Mixing the melted paint evenly and keeping it warm for 3-5 mins before marking the road |
F. Allow primer to dry before applying paint |
G. Primer is applied a few wider than the width of the thermoplastic n> |
H. New aslt and concrete must be allowed to cure for a minimum of 30 days before applying paint |