High purity iron billet,electric steel, electric magnetic iron, ultra low carbon magnetic iron bar,soft magnetic iron bar SUYB-1, Pure iron(SAE AMS 7707C Iron) ingot iron, iron billet,soft iron, Armco Pure iron, iron remelt ingot, Melting Grade Pure Iron Billetï¼ASTM A848 magnetic iron(alloy 1), Iron Cathode, electrolytic iron were supplied by us, The chemical composition and sics characteristics, such as the coercive force is better than the International Standard. Our fabrication plant is equipped with large cutting machine, shearing machine, sawing machine, punch, lathe, mill machine, annealing furnace, and rattle barrel to meet the different needs of users. We check and audit the quality according to the quality certificate strictly
Trademark B-A
Chemical composition %,max
C 0.003 Si 0.01 Mn 0.20 P 0.012 S 0.006 Al 0.15-0.50 Cr 0.02 Ni 0.01 Cu 0.02
Trademark B-AA
Chemical composition %,max
C 0.002 Si 0.006 Mn 0.12 P 0.007 S 0.001 Al 0.15-0.50 Cr 0.02 Ni 0.01 Cu 0.005
Trademark B-B:
C 0.003 Si 0.01 Mn 0.13 P 0.009 S 0.006 Cr 0.02 Ni 0.02 Al 0.03 Cu 0.02
Trademark B-BC:
C 0.002 Si 0.01 Mn 0.08 P 0.006 S 0.005 Cr 0.01 Ni 0.01 Al 0.01 Cu 0.01
Trademark B-CC:
C 0.002 Si 0.003 Mn 0.02 P 0.005 S 0.005 Cr 0.01 Ni 0.01 Al 0.005 Cu 0.004
Trademark B-EA:
C 0.002 Si 0.005 Mn 0.0005 P 0.001 S 0.0002 Cr 0.001 Ni 0.005 Al 0.002 Cu 0.0005
Type mm : Medium plate and steel billet 8-250 ,plate coil 12-25 ,straight round steel dia6.5-dia300 ,round steel coil,cold drawn plate coil 0.5-2.5 tube,etc. We can produce the special type which you ask
application:
a.make it in electric core.heel piece, gag bit in electric appliance device,telecommunication
b.Electric core of electric iron
c.Electromagnetic part of instruments and meters
d.Iron core and shell of direct-current dynamo
e.Electric part or magnetic part for car,tractor,lathe
f.Magnetic shielding apparatus
Charateristic
Mechanical Properties
Brinell Hardness (HB) |
| |
HIGH PURITY IRON | max. | typical |
Cold-rolled strip / sheet | 105 | 90 |
Hot-rolled strip / plate | 105 | 90 |
Quarto plate | 100 | 90 |
Round bar | 110 | 95 |
Electrical and Magnetic Properties Characteristics Typical Values
Initial Permeability | 300 â 500 |
Permeability | 3500 - 6000 |
Coercive Force | 60 â 120 A/m |
Saturation Induction | 2.15 T |
Density at 20 °C | 7.86 kg/dm³ |
Melting Point | 1536 °C |
pansion Coefficient Temperature Range 0 â 100 °C | 12x10-6 1/°C |
Modulus of Elasticity | 207 kN/mm² |