If you put in boiling water for 48 hours, it's still viscose and undeformed.The sical performance is better than the iron mold, which can meet the requirements of the mold structure. The iron parts are easy to deform and even difficult to restore flatness after repair.
It is good to achieve higher economic benefits.It is especially suitable for pouring concrete, which can make the surface of concrete smooth.
Solve the problem of water leakage and rough surface during construction.
The cost is greatly reduced and the corrosion and corrosion of iron mould are avoided
If used strictly in accordance with illustrations, can be reused more than 50 times